金属学报. 2017, 53 (5): 567-574 doi: 10.11900/0412.1961.2016.00307



焊接温度对碳钢/奥氏体不锈钢扩散焊接头界面组织及性能的影响
王大伟,修世超

Effect of Bonding Temperature on the Interfacial Micro-structure and Performance of Mild Steel/Austenite Stainless Steel Diffusion-Bonded Joint
Dawei WANG,Shichao XIU
图5 不同焊接温度Q235A低碳钢/AISI304不锈钢扩散焊界面显微硬度分布
Fig.5 Microhardness distributions of the Q235A mild steel/AISI304 stainless steel diffusion-boned interface at different temperatures