金属学报. 2017, 53 (5): 567-574 doi: 10.11900/0412.1961.2016.00307



焊接温度对碳钢/奥氏体不锈钢扩散焊接头界面组织及性能的影响
王大伟,修世超

Effect of Bonding Temperature on the Interfacial Micro-structure and Performance of Mild Steel/Austenite Stainless Steel Diffusion-Bonded Joint
Dawei WANG,Shichao XIU
图2 不同温度焊接时Q235A低碳钢/AISI304不锈钢扩散焊接头OM像
Fig.2 OM images of the Q235A mild steel/AISI304 stainless steel diffusion-boned joint at different temperatures (I—ferrite and pearlite, II—single ferrite, III—fine-grained austenite, IV—coarse-grained austenite) (a) 800 ℃ (b) 850 ℃ (c) 900 ℃