金属学报. 2017, 53 (5): 567-574 doi: 10.11900/0412.1961.2016.00307



焊接温度对碳钢/奥氏体不锈钢扩散焊接头界面组织及性能的影响
王大伟,修世超

Effect of Bonding Temperature on the Interfacial Micro-structure and Performance of Mild Steel/Austenite Stainless Steel Diffusion-Bonded Joint
Dawei WANG,Shichao XIU
图1 焊接温度850 ℃时Q235A低碳钢/AISI304不锈钢扩散焊界面附近区域的EBSD像
Fig.1 EBSD image near the Q235A mild steel/AISI304 stainless steel diffusion-bonding interface at welding temperature of 850 ℃ (Green line: small angle grain boundary, θ=2°~15°.Black line: high angle grain boundary, θ>15°)