金属学报. 2017, 53 (5): 549-558 doi:
10.11900/0412.1961.2016.00316
中厚板表层超细晶对止裂性能的影响
马江南,王瑞珍,杨才福,查小琴,张利娟
Effect of Surface Layer with Ultrafine Grains on Crack Arrestability of Heavy Plate
Jiangnan MA,Ruizhen WANG,Caifu YANG,Xiaoqin ZHA,Lijuan ZHANG
图3 TRRP钢和TMCP钢表层冲击吸收功随温度的变化
Fig.3 Charpy absorbed energy
vs
temperature of TRRP (a) and TMCP (b) steels