金属学报. 2017, 53 (5): 549-558 doi: 10.11900/0412.1961.2016.00316



中厚板表层超细晶对止裂性能的影响
马江南,王瑞珍,杨才福,查小琴,张利娟

Effect of Surface Layer with Ultrafine Grains on Crack Arrestability of Heavy Plate
Jiangnan MA,Ruizhen WANG,Caifu YANG,Xiaoqin ZHA,Lijuan ZHANG
图10 TRRP钢和TMCP钢表层组织的取向成像图和取向差分布图
Fig.10 Misorientation maps (a, c) and misorientation angle distribution diagrams (b, d) of surface layer of TRRP (a, b) and TMCP (c, d) steels (In Figs.10a and c, black lines show grain boundaries larger than 15°, red lines show grain boundaries between 2°and 15°)