金属学报. 2017, 53 (5): 531-538 doi: 10.11900/0412.1961.2016.00321



热加工对Z3CN20-09M双相不锈钢组织及热老化冲击断裂行为的影响
张海,李时磊,刘刚,王艳丽

Effects of Hot Working on the Microstructure and Thermal Ageing Impact Fracture Behaviors of Z3CN20-09MDuplex Stainless Steel
Hai ZHANG,Shilei LI,Gang LIU,Yanli WANG
图6 铸态和锻态Z3CN20-09M双相不锈钢Charpy冲击功随热老化时间的变化趋势
Fig.6 Change of Charpy-impact energy with ageing time for Z3CN20-09M duplex stainless steel before and after 20% hot forged reduction+solution treatment at 1050 ℃ for 1 h