金属学报. 2017, 53 (5): 531-538 doi: 10.11900/0412.1961.2016.00321



热加工对Z3CN20-09M双相不锈钢组织及热老化冲击断裂行为的影响
张海,李时磊,刘刚,王艳丽

Effects of Hot Working on the Microstructure and Thermal Ageing Impact Fracture Behaviors of Z3CN20-09MDuplex Stainless Steel
Hai ZHANG,Shilei LI,Gang LIU,Yanli WANG
图2 Z3CN20-09M双相不锈钢铸态及热锻态的EBSD像
Fig.2 EBSD images of Z3CN20-09M duplex stainless steel before (a) and after 20% hot forged reduction (b)