热加工对Z3CN20-09M双相不锈钢组织及热老化冲击断裂行为的影响 |
Effects of Hot Working on the Microstructure and Thermal Ageing Impact Fracture Behaviors of Z3CN20-09MDuplex Stainless Steel |
图10 Z3CN20-09M双相不锈钢中取向相同的铁素体在断裂时形成的解理小平面 |
Fig.10 Cleavage facets formed by fracturing of ferrites with the same orientation (as circled by yollow lines) in Z3CN20-09M duplex stainless steel |
![]() |