TA1/X65复合板焊接工艺及焊缝组织和性能研究*
毕宗岳1,2(),杨军1,2,刘海璋1,2,张万鹏1,2,杨耀彬1,2,田磊1,2,黄晓江1,2
INVESTIGATION ON THE WELDING PROCESS AND MICROSTRUCTURE AND MECHANICAL PROPERTY OF BUTT JOINTS OF TA1/X65 CLAD PLATES
Zongyue BI1,2(),Jun YANG1,2,Haizhang LIU1,2,Wanpeng ZHANG1,2,Yaobin YANG1,2,Lei TIAN1,2,Xiaojiang HUANG1,2

图4. 焊缝各区域的XRD谱

Fig.4. XRD spectra of weld zones in joint in Fig.2 (s,s—solid solution)

(a) transition interface of areas 1 and 2 (b) transition interface of areas 2 and 3 (c) transition interface of areas 3 and 4