等温淬火低合金贝氏体球墨铸铁的回火组织与力学性能*
崔君军1,陈礼清1(),李海智2,佟伟平2
TEMPERED MICROSTRUCTURE AND MECHANICAL PROPERTIES OF AUSTEMPERED LOW ALLOYED BAINITIC DUCTILE IRON
Junjun CUI1,Liqing CHEN1(),Haizhi LI2,Weiping TONG2

图3. 等温淬火低合金贝氏体球墨铸铁中马氏体的TEM像和选区电子衍射花样及标定

Fig.3. Low (a) and high magnified (b) TEM images of martensite of low alloyed austempered bainite ductile iron (Inset in Fig.3a show the selected area electron diffraction (SAED) pattern along [110] zone axis, T—twin crystal)