合金成分和冷却速率对Al-Cu合金凝固过程中初生Al2Cu相生长形貌的影响*
|
EFFECT OF ALLOY COMPOSITION AND COOLING RATE ON THE GROWTH MORPHOLOGY OF PRIMARY Al2Cu PHASE IN Al-Cu ALLOY DURING SOLIDIFICATION
|
图7. Al-45%Cu合金横截面初生Al2Cu相形貌转变示意图 |
Fig 7. chematic of primary Al2Cu phase morphology transition in Al-45%Cu alloy cross section |
![]() |