7050铝合金淬火敏感性研究和微观组织分析*
|
RESERCH ON QUENCH SENSITIVITY AND MICROSTRUCTURE ANALYSIS OF 7050 ALUMINUM ALLOY
|
图3. 7050铝合金等温保温过程的时间-温度-转化率(TTT)曲线 |
Fig.3. Time-temperature-transformation (TTT) curves of 7050 aluminum alloy during isothermal holding process |
![]() |