连续SiC纤维增强钛基复合材料研究进展*
|
ADVANCES IN SiC FIBER REINFORCED TITANIUM MATRIX COMPOSITES
|
图1. 直流加热法和射频加热法SiC纤维生产示意图 |
Fig.1. Schematic diagrams of SiC fiber production bydirect current heating method (a) and radio frequency heating method (b) |
![]() |