汽车用新型Al-0.93Mg-0.78Si-0.20Cu-3.00Zn合金的制备及其时效析出行为研究*
|
PRECIPITATION BEHAVIORS AND PREPARATION OF AN ADVANCED Al-0.93Mg-0.78Si-0.20Cu-3.00Zn ALLOY FOR AUTOMOTIVE APPLICATION
|
图6. Al-0.93Mg-0.78Si-0.20Cu-3.00Zn合金不同状态下的工程应力-应变曲线 |
Fig.6. Engineering stress-strain curves of the Al-0.93Mg-0.78Si-0.20Cu-3.00Zn alloy in the different conditions |
![]() |