深海环境中的材料腐蚀与防护研究进展
曹攀, 周婷婷, 白秀琴, 袁成清

Research Progress on Corrosion and Protection in Deep-sea Environment
CAO Pan, ZHOU Tingting, BAI Xiuqin, YUAN Chengqing
表1 南海海水环境因素数据[6]
Table 1 Environmental factors of sea water at South China Sea[6]
Depth
m
Temperature
Salinity
Oxygen
mgL-1
300 10.8 34.4 3.46
500 8.0 34.4 2.66
800 5.2 34.5 2.48
1200 3.4 34.6 2.66
2000 2.5 34.6 2.96
3000 2.4 34.6 3.20