阳极氧化电压对钛合金TC4阳极氧化TiO2膜层表面的影响*
严继康1,2,杨钢1(),唐婉霞1,2,吴云峰1,方树铭1,施哲3
Effect of Applied Voltage on Performance of Anodic Oxidation Films of TiO2 on TC4 Alloy
Jikang YAN1,2,Gang YANG1,**(),Wanxia TANG1,2,Yunfeng WU1,Shuming FANG1,Zhe SHI3

图4. 不同氧化电压TC4阳极氧化膜表面的SEM像

Fig.4. SEM images of surface of films on TC4 for different oxygen voltage, (a) 30 V, (b) 70 V, (c) 100 V