纳米纤维素/阳离子聚合物复合三维组织工程支架的性能*
唐爱民(),刘远,赵姗
Performance of 3D Tissue Engineering Scaffolds of Nanocellulose/High Cationic Polymers Composite
Aimin TANG(),Yuan LIU,Shan ZHAO

图4. 液体置换法测定的纳米纤维素分别与聚合物A、B复合支架的孔隙率

Fig.4. Porosity measured by liquid displacement experiment for nanocellulose/polymer A and nanocellulose/polymer B compound scaffolds