原油含水率对油气管材超临界CO2腐蚀行为的影响
|
Effect of Water Content of Crude Oil on Corrosion Behavior of Oil and Gas Tubular Goods Steel in Supercritical CO2 System
|
图3. N80钢腐蚀产物膜表面SEM像 |
Fig.3. SEM images of surface corrosion scales on N80 steel water cut: (a) 30%, (b) 50%, (c) 75%, (d) 90% |
![]() |