防锈油不同涂油量对冷轧钢板腐蚀行为的影响
|
|
Effect of Different Amounts of Antirust Oil on Corrosion Behavior of Cold-rolled Steel
|
|
图9. 防锈油膜试样在5%NaCl溶液中浸泡不同时间的Mott-Schottky图 |
Fig.9. Mott-Schottky plots of oil-coated steels in 5%NaCl solution after immersion for 0 h (a), 4 h (b) and 8 h (c) |
![]() |