Al-Mg-Sn-Si-In铝合金在不同溶液中的腐蚀与电化学性能研究
|
Corrosion and Electrochemical Performance of Al-Mg-Sn-Si-In Alloy in Different Solutions
|
图2. Al-0.5Mg-0.1Sn-0.1Si-0.02In合金在3种溶液中及纯Zn在溶液2中的恒流放电曲线 |
Fig.2. Discharge behavior of metal-air battery based on Al-0.5Mg-0.1Sn-0.1Si-0.02In alloy in 2 mol/L NaCl, 4 mol/L NaOH ethanol-10% water, 4 mol/L NaOH solutions and Zn in 4 mol/L NaOH solution |
![]() |