熔模铸造条件下Ti6Al4V合金铸件与陶瓷型壳间界面换热系数研究*
|
RESEARCH ON THE INTERFACIAL HEAT TRANSFER COEFFECIENT BETWEEN CASTING AND CERAMIC SHELL IN INVESTMENT CASTING PROCESS OF Ti6Al4V ALLOY
|
图2. 铸型型腔形状及热电偶布置示意图 |
Fig.2. Schematic of the cavity and the positions of the thermocouples (TC) |
![]() |