熔模铸造条件下Ti6Al4V合金铸件与陶瓷型壳间界面换热系数研究*
|
RESEARCH ON THE INTERFACIAL HEAT TRANSFER COEFFECIENT BETWEEN CASTING AND CERAMIC SHELL IN INVESTMENT CASTING PROCESS OF Ti6Al4V ALLOY
|
图4. Ti6Al4V合金的c和导热系数l随温度的变化 |
Fig.4. Variations of c (a) and thermal conductivity l (b) of Ti6Al4V with temperatures |
![]() |