Cu-Co-Fe合金雾化合金液滴凝固过程研究*
赵雷1,2,江鸿翔2,AHMAD Tauseef2,赵九洲2()
STUDY OF SOLIDIFICATION FOR GAS-ATOMIZED DROPLET OF Cu-Co-Fe ALLOY
Lei ZHAO1,2,Hongxiang JIANG2,Tauseef AHMAD2,Jiuzhou ZHAO2()

图1. 不同直径Cu-10%Co-10%Fe合金粉末的SEM像和数量密度分布

Fig.1. SEM images of Cu-10%Co-10%Fe powders with diameters of 88~100 mm (a), 125~150 μm (b), 200~220 mm (c) and distribution of number density (N) of Fe-Co-rich phase particles along radial direction (r) of the Cu-10%Co-10%Fe powder with diameter of 125~150 mm (d)