[an error occurred while processing this directive]
晶体相场法研究Kirkendall效应诱发的相界空洞的形成和演变*
卢艳丽(),卢广明,胡婷婷,杨涛,陈铮
PHASE FIELD CRYSTAL STUDY ON THE FORMATION AND EVOLUTION OF PHASE BOUNDARY VOID INDUCED BY THE KIRKENDALL EFFECT
Yanli LU(),Guangming LU,Tingting HU,Tao YANG,Zheng CHEN

图 5. MA=100MB时不同相界取向差角扩散体系中自由能随时间的变化

Fig.5. Free energy evolution curves corresponding to different misorientations for the same atomic mobility ratio (MA=100MB)