Si对高Nb-TiAl合金组织及室温拉伸性能的影响*
|
|
EFFECT OF Si ADDITION ON THE MICROSTRUCTURE AND ROOM TEMPERATURE TENSILE PROPERTIES OF HIGH Nb-TiAl ALLOY
|
|
图3. HT3试样中析出相的TEM像、SAED谱及HRTEM像 |
Fig.3. TEM images and SAED patterns (insets) of e2 phase (a) and e3 phase (b) in sample HT3, and HRTEM image of the e3/g interface (c) (The corresponding FFT image is shown in the lower right, the inverse FFT image of interface dislocation is shown in the upper right in Fig.3c) |
![]() |