脉冲磁场作用下矩形截面宽厚比对K4169高温合金晶粒细化的影响*
|
|
EFFECT OF RECTANGLE ASPECT RATIO ON GRAIN REFINEMENT OF SUPERALLOY K4169 UNDER PULSED MAGNETIC FIELD
|
|
图2. 矩形截面试件(宽厚比为5.5)的三维有限元模型及网格划分 |
Fig.2. 3D FEM model and mesh of rectangular sample with aspect ratio of 5.5 |
![]() |