脉冲磁场作用下矩形截面宽厚比对K4169高温合金晶粒细化的影响*
|
|
EFFECT OF RECTANGLE ASPECT RATIO ON GRAIN REFINEMENT OF SUPERALLOY K4169 UNDER PULSED MAGNETIC FIELD
|
|
图8. 宽厚比为1.0的试件中心轴高度75 mm处的节点流速随时间的演变规律 |
Fig.8. Evolution of fluid rate at 75 mm height on central axis of the sample with aspect ratio of 1.0 (Inset shows the fluid rate in 5 pulse periods between 25 s and 26 s) |
![]() |