脉冲磁场作用下矩形截面宽厚比对K4169高温合金晶粒细化的影响*
|
|
EFFECT OF RECTANGLE ASPECT RATIO ON GRAIN REFINEMENT OF SUPERALLOY K4169 UNDER PULSED MAGNETIC FIELD
|
|
图5. 激励电流峰值时刻及下降期空间磁感应强度的分布 |
Fig.5. Distributions of magnetic flux density at peak value of excitation current (a) and descending stage of excitation current (b) |
![]() |