脉冲磁场作用下矩形截面宽厚比对K4169高温合金晶粒细化的影响*
|
|
EFFECT OF RECTANGLE ASPECT RATIO ON GRAIN REFINEMENT OF SUPERALLOY K4169 UNDER PULSED MAGNETIC FIELD
|
|
图6. 激励电流峰值时刻和激励电流下降期的感应电流密度和电磁力的分布(各小图为中心横截面上相应的分布) |