EFFECT OF Zr ADDITION ON MICROSTRUCTURE AND MECHANICAL PROPERTIES OF NiAl/Cr(Mo) BASE EUTECTIC ALLOY
Liyuan SHENG
1
(
),Jianting GUO
2
,Chen LAI
1
,Tingfei XI
1
图2. A1和A4合金的XRD谱
Fig.2. XRD spectra of A1 and A4 alloys