合金元素Hf, Sn, Ta, Zr, Dy和Ho对Nb-Nb5Si3合金组织和力学性能的影响*
|
|
EFFECT OF Hf, Sn, Ta, Zr, Dy AND Ho ON MICRO- STRUCTURE AND MECHANICAL PROPERTIES OF Nb-Nb5Si3 ALLOY
|
|
图14. Nb-23Ti-10Ta-2Cr-18Si-xDy合金的BSE像[13] |
Fig.14. BSE images of Nb-23Ti-10Ta-2Cr-18Si-xDy alloy with x=0 (a) and x=0.1 (b) [13] |
![]() |