		合金元素Hf, Sn, Ta, Zr, Dy和Ho对Nb-Nb5Si3合金组织和力学性能的影响*
		 | 
| 
			EFFECT OF Hf, Sn, Ta, Zr, Dy AND Ho ON MICRO- STRUCTURE AND MECHANICAL PROPERTIES OF Nb-Nb5Si3 ALLOY
			 | 
| 图12. Zr含量对Nb-22Ti-16Si合金室温压缩性能的影响[11] | 
| Fig.12. Compressive properties of Nb-22Ti-16Si alloys with different Zr contents[11] | 
|  |