合金元素Hf, Sn, Ta, Zr, Dy和Ho对Nb-Nb5Si3合金组织和力学性能的影响*
|
|
EFFECT OF Hf, Sn, Ta, Zr, Dy AND Ho ON MICRO- STRUCTURE AND MECHANICAL PROPERTIES OF Nb-Nb5Si3 ALLOY
|
|
图8. 不同Ta含量Nb-22Ti-16Si-7Cr-3Al合金在1000 ℃的压缩屈服强度[13] |
Fig.8. Compressive yield strength for Nb-22Ti-16Si-7Cr-3Al alloy with different Ta contents at 1000 ℃[13] |
![]() |