		合金元素Hf, Sn, Ta, Zr, Dy和Ho对Nb-Nb5Si3合金组织和力学性能的影响*
		 | 
| 
			EFFECT OF Hf, Sn, Ta, Zr, Dy AND Ho ON MICRO- STRUCTURE AND MECHANICAL PROPERTIES OF Nb-Nb5Si3 ALLOY
			 | 
| 图3. Nb-16Si-1Hf合金的裂纹扩展路线形貌[10] | 
| Fig.3. Morphologies of crack propagation through bridging (a) and deflection (b) of Nb-16Si-1Hf alloy [10] | 
|  |