		合金元素Hf, Sn, Ta, Zr, Dy和Ho对Nb-Nb5Si3合金组织和力学性能的影响*
		 | 
| 
			EFFECT OF Hf, Sn, Ta, Zr, Dy AND Ho ON MICRO- STRUCTURE AND MECHANICAL PROPERTIES OF Nb-Nb5Si3 ALLOY
			 | 
| 图19. Nb-22Ti-16Si-7Cr-3Al-3Ta-2Hf-0.1Ho合金横截面和纵截面的BSE像[19] | 
| Fig.19. BSE images of Nb-22Ti-16Si-7Cr-3Al-3Ta-2Hf-0.1Ho alloy in transverse (a) and longitudinal (b) sections[19] | 
|  |