纳米Al2O3和NiAl共同强化的铁基ODS合金的铝热合成研究
|
|
Al2O3 NANOPARTICLE AND NiAl REINFORCED Fe-BASED ODS ALLOYS SYNTHESIZED BY THERMITE REACTION
|
|
图9. 添加不同TiO2凝胶含量的铝热合成铁基ODS合金的拉伸断口的SEM像 |
Fig.9. SEM images of fractographs of Fe-based ODS alloys synthesized by themite reaction process with addition of 0 (a), 0.87% (b), 1.24% (c) and 1.98% (d) TiO2 xerogel |
![]() |