Al2O3 NANOPARTICLE AND NiAl REINFORCED Fe-BASED ODS ALLOYS SYNTHESIZED BY THERMITE REACTION
|
|
图5. 添加不同TiO2凝胶含量的铝热合成铁基ODS合金的SEM像 |
Fig.5. SEM images of Fe-based ODS alloys synthesized by thermite reaction process with addition of 0 (a, b), 0.87% (c, d), 1.24% (e, f) and 1.98% (g, h) TiO2 xerogel at low (a, c, e, g) and high (b, d, f, h) magnification |
![]() |