纳米Al2O3和NiAl共同强化的铁基ODS合金的铝热合成研究
|
|
Al2O3 NANOPARTICLE AND NiAl REINFORCED Fe-BASED ODS ALLOYS SYNTHESIZED BY THERMITE REACTION
|
|
图8. TiO2凝胶含量对铝热合成铁基ODS合金拉伸强度和断后伸长率的影响 |
Fig.8. Effect of different contents of TiO2 xerogel on tensile strength and elongation for Fe-based ODS alloys synthesized by thermite reaction process |
![]() |