纳米Al2O3和NiAl共同强化的铁基ODS合金的铝热合成研究
|
|
Al2O3 NANOPARTICLE AND NiAl REINFORCED Fe-BASED ODS ALLOYS SYNTHESIZED BY THERMITE REACTION
|
|
图7. 不同TiO2凝胶含量铝热合成铁基ODS合金的应力-应变曲线 |
Fig.7. Stress-strain curves for Fe-based ODS alloys synthesized by thermite reaction process with different contents of TiO2 xerogel addition |
![]() |