超快冷终冷温度对含Nb-V-Ti微合金钢组织转变及析出行为的影响*
|
|
EFFECT OF FINAL TEMPERATURE AFTER ULTRA-FAST COOLING ON MICROSTRUCTURAL EVOLUTION AND PRECIPITATION BEHAVIOR OF Nb-V-Ti BEARING LOW ALLOY STEEL
|
|
图6. 实验钢超快冷至不同温度时基体的屈服强度及析出强化增量 |
Fig.6. Yield strength of matrix and the contribution of precipitation strength to yield strength of the experimental steel after UFC to different temperatures |
![]() |