超快冷终冷温度对含Nb-V-Ti微合金钢组织转变及析出行为的影响*
|
|
EFFECT OF FINAL TEMPERATURE AFTER ULTRA-FAST COOLING ON MICROSTRUCTURAL EVOLUTION AND PRECIPITATION BEHAVIOR OF Nb-V-Ti BEARING LOW ALLOY STEEL
|
|
图1. 超快冷至不同温度的缓冷与动态连续冷却工艺曲线图 |
Fig.1. Curves of ultra-fast cooling (UFC) to different temperatures and dynamic continuous cooling transformation (CCT) (F—ferrite, P—pearlite, AF—acicular ferrite, B—bainite, M—martensite, CR—cooling rate) |
![]() |