超细晶粒钢中晶粒尺寸对塑性的影响模型*
|
|
MODEL OF THE EFFECT OF GRAIN SIZE ON PLASTI-CITY IN ULTRA-FINE GRAIN SIZE STEELS
|
|
图4. 晶界阻碍Frank-Read源(FR源)增殖产生位错的示意图 |
Fig.4. Schematic of grain boundary blocks the process of Frank-Read source (FR source) emits dislocations (Both da and db represent grain size and da>db) |
![]() |