取向硅钢中 114 418 织构对二次再结晶时晶粒异常长大的影响*
刘志桥,杨平(),毛卫民,崔凤娥
EFFECT OF 114 418 TEXTURE ON ABNORMAL GROWTH DURING SECONDARY RECRYSTALLI- ZATION IN GRAIN-ORIENTED STEEL
Zhiqiao LIU,Ping YANG(),Weimin MAO,Feng'e CUI

图2. 初次再结晶后样品的EBSD取向成像图

Fig.2. EBSD orientation images of primary recrystallization sample

(a) orientation distribution (b) ODF, φ2=45°