[an error occurred while processing this directive]
取向硅钢中 114 418 织构对二次再结晶时晶粒异常长大的影响*
刘志桥,杨平(),毛卫民,崔凤娥
EFFECT OF 114 418 TEXTURE ON ABNORMAL GROWTH DURING SECONDARY RECRYSTALLI- ZATION IN GRAIN-ORIENTED STEEL
Zhiqiao LIU,Ping YANG(),Weimin MAO,Feng'e CUI

图1. 冷轧板的EBSD取向成像图

Fig.1. EBSD orientation images of cold-rolled sample

(a) orientation distribution map (ND—normal direction, RD—rolling direction)

(b) {100} pole figure (TD—transverse direction)

(c) orientation distribution function (ODF), φ2=45°