Al-7Si-Mg合金凝固过程形核模型建立及枝晶生长过程数值模拟*
陈瑞1,许庆彦1(),吴勤芳2,郭会廷2,柳百成1
NUCLEATION MODEL AND DENDRITE GROWTH SIMULATION IN SOLIDIFICATON PROCESS OF Al-7Si-Mg ALLOY
Rui CHEN1,Qingyan XU1(),Qinfang WU2,Huiting GUO2,Baicheng LIU1

图9. 模拟获得的No.2, No.4, No.6和No.7测温点处的最终凝固组织

Fig.9. Simulated final dendrite microstructures of the positions No.2 (a), No.4 (b), No.6 (c) and No.7 (d) (Different colors represent different dendrites)