Al-7Si-Mg合金凝固过程形核模型建立及枝晶生长过程数值模拟*
|
|
NUCLEATION MODEL AND DENDRITE GROWTH SIMULATION IN SOLIDIFICATON PROCESS OF Al-7Si-Mg ALLOY
|
|
图12. 凝固结束时二维截面枝晶形貌和实验结果对比 |
Fig.12. Simulated final dendrite morphologies on arbitrarily two dimensional sections (a) and the obtained experimental metallographic microstructure solidified at the position of No.7 (b) |
![]() |