激光+GMAW复合热源焊熔池流体流动的数值分析*
|
NUMERICAL ANALYSIS OF FLUID FLOW IN LASER+GMAW HYBRID WELDING
|
图9. 激光功率为2000 W时不同时刻复合焊熔池横截面的温度场和流场分布 |
Fig.9. Temperature and flow fields at cross section of weld pool in hybrid welding for 0.44 s (a), 0.5 s (b), 0.8 s (c) and 1.2 s (d) with PL=2000 W and x=20 mm |
![]() |