Mo含量对CrMoN复合涂层的组织结构和性能的影响
|
|
齐东丽, 雷浩, 范迪, 裴志亮, 宫骏, 孙超
|
EFFECT OF Mo CONTENT ON THE MICROSTRUC-TURE AND PROPERTIES OF CrMoN COMPOSITE COATINGS
|
|
QI Dongli, LEI Hao, FAN Di, PEI Zhiliang, GONG Jun, SUN Chao
|
|
| 表1 CrMoN复合涂层沉积参数 |
| Table 1 Deposition conditions for CrMoN composite coatings |
|
Sample No. | Process | Gas flow rate / (mL·min-1) | Cr target current / A | Mo target current / A | Substrate bias / V | Time min | | Ar | N2 | | Substrate cleaning | 60 | - | 0.4 | - | -200 | 5 | | Cr adhesion layer | 60 | - | 0.4 | - | -100 | 5 | | 1 | CrN | 30 | 30 | 0.4 | - | -100 | 60 | | 2 | CrMoN | 30 | 30 | 0.4 | 0.2 | -100 | 120 | | 3 | CrMoN | 30 | 30 | 0.4 | 0.3 | -100 | 120 | | 4 | CrMoN | 30 | 30 | 0.4 | 0.4 | -100 | 120 | | 5 | CrMoN | 30 | 30 | 0.3 | 0.4 | -100 | 120 | | 6 | CrMoN | 30 | 30 | 0.2 | 0.4 | -100 | 120 |
|
|
|