Zn-Al钎料成分对Cu/Zn-Al/Al钎焊接头界面结构及性能的影响
|
|
羊浩, 黄继华, 陈树海, 赵兴科, 王奇, 李德华
|
INFLUENCE OF THE COMPOSITION OF Zn-Al FILLER METAL ON THE INTERFACIAL STRUCTURE AND PROPERTY OF Cu/Zn-Al/Al BRAZED JOINT
|
|
YANG Hao, HUANG Jihua, CHEN Shuhai, ZHAO Xingke, WANG Qi, LI Dehua
|
|
| 表2 图2中Cu/Al接头界面区物相的EDS分析结果 |
| |
|
| Filler metal | Position | Atomic fraction / % | Possible phase | | Al | Cu | Zn | | Zn-15Al | A | 55.15 | 34.12 | 10.23 | Al4.2Cu3.2Zn0.7 | | Zn-22Al | B | 55.00 | 35.96 | 9.03 | Al4.2Cu3.2Zn0.7 | | C | 68.34 | 28.26 | 3.40 | CuAl2 | | Zn-28Al | D | 53.77 | 35.34 | 10.89 | Al4.2Cu3.2Zn0.7 | | E | 67.88 | 26.77 | 5.35 | CuAl2 | | Zn-37Al | F | 55.14 | 37.59 | 7.27 | Al4.2Cu3.2Zn0.7 | | G | 67.99 | 29.25 | 2.77 | CuAl2 | | Zn-45Al | H | 56.33 | 38.50 | 5.17 | Al4.2Cu3.2Zn0.7 | | I | 69.09 | 28.94 | 1.96 | CuAl2 |
|
|
|