耦合孪生的TWIP钢单晶体塑性变形行为模拟研究
孙朝阳, 郭祥如, 黄杰, 郭宁, 王善伟, 杨竞

MODELLING OF PLASTIC DEFORMATION ON COUPLING TWINNING OF SINGLE CRYSTAL TWIP STEEL
SUN Chaoyang, GUO Xiangru, HUANG Jie, GUO Ning, WANG Shanwei, YANG Jing
表2 TWIP钢12个孪生系的孪生面和孪生方向
Table 2 Twinning planes and twinning directions for TWIP steel with 12 twinning systems
Twinning system Twinning plane Twinning direction Twinning system Twinning plane Twinning direction
t1 ( 111 ) [ 11 2 ? ] u1 ( 1 ? 1 ? 1 ) [ 112 ]
t2 ( 111 ) [ 2 ? 1 1 ] u2 ( 1 ? 1 ? 1 ) [ 2 1 ? 1 ]
t3 ( 111 ) [ 1 2 ? 1 ] u3 ( 1 ? 1 ? 1 ) [ 1 ? 21 ]
v1 ( 1 ? 11 ) [ 211 ] w1 ( 1 1 ? 1 ) [ 121 ]
v2 ( 1 ? 11 ) [ 1 2 1 ? ] w2 ( 1 1 ? 1 ) [ 2 1 1 ? ]
v3 ( 1 ? 11 ) [ 1 1 ? 2 ] w3 ( 1 1 ? 1 ) [ 1 ? 1 2 ]